Electron Backscatter Diffraction (EBSD)

OIM study of fractured electron beam welds in Beryllium.

S.I. Wright and J.D. Cotton (1995). "Microtextural Characterization of a Beryllium Weldment." Textures and Microstructures 23:7-19.

EDAX Periodic Table of Elements - Beryllium

OIM orientation map of a fractured e-beam welded Beryllium sample with
a corresponding optical microscopy image