Skip to content

Uranium

Electron Backscatter Diffraction (EBSD)

Deformation Twins in Hydrided α-Uranium

(Textures, in gray scale, shown with matrix orientations removed)

EDAX Periodic Table of Elements - Uranium

EDAX Periodic Table of Elements - Uranium

EDAX Periodic Table of Elements - Uranium

J. F. Bingert, R. J. Hanrahan, Jr., R. D. Field and P. O. Dickerson (2003). "Microtextural investigation of Hydrided α-Uranium." Journal of Alloys and Compounds 365: 138-148.

Micro X-ray Fluorescence (Micro-XRF)

EDAX Periodic Table of Elements - Uranium
Analysis results for a uranium glass sample. Red – with no barrier; blue – enclosed in a single 50 um bag; green – enclosed in two layers of 50 um bag.

EDAX Periodic Table of Elements - Uranium
Analysis results for a Canmet DH-1 sample. Red – enclosed in thin Mylar envelope; blue – enclosed in 50 um plastic bag; green – enclosed in 50 um plastic bag using rhodium primary beam filter.