The Sapphire Si(Li) Detecting Unit with Classic 10-Liter Dewar Style

Overview

Only EDAX offers the Sapphire detector with such an advanced specification for light element performance. The light element sensitivity is superior to any other offering on the market today. The Sapphire process has provided the best crystal manufacturing in quality and consistency, enabling EDAX to pass on to our customers the benefits of these high yields. The Sapphire Si(Li) DU offers:

  • Super Ultra Thin window technology, for superior light element analysis down to Beryllium
  • 10mm2 or 30mm2 detector crystals to suit any application
  • Industry leading peak-to-background ratio
classic 10-liter
 