Microstructure of a Stainless Steel Golf Club Head

Collected by Matt Nowell, EDAX

Microstructure of a Stainless Steel Golf Club Head

This orientation map is from a 17-4 stainless-steel golf club. This microstructure consists of a proeutectoid cementite network surrounding pearlite colonies.